Dear Saleem,
When planning to perform a Procedure Qualification Record (PQR) and develop a Welding Procedure Specification (WPS) using the E11018M electrode, it's essential to select an appropriate base material. The E11018M electrode is a low-hydrogen, iron-powder type electrode that is designed for welding high-strength steels.
For the E11018M electrode, you should choose materials that are compatible with the high-strength, low-alloy properties of the electrode. Here are some suggestions:
ASTM A514 (T-1) Steel:
ASTM A517 Steel:
ASTM A710 Steel:
ASTM A709 Grade 100/100W:
ASTM A572 Grade 100:
HY-80, HY-100:
When selecting the material, consider the specific requirements of your application, such as strength, toughness, and environmental conditions. Ensure that the material's mechanical properties are compatible with the E11018M electrode's characteristics.
For welding with the E11018M electrode, you should use high-strength, low-alloy steels such as ASTM A514, ASTM A517, ASTM A710, ASTM A709 Grade 100/100W, ASTM A572 Grade 100, or HY-80/HY-100. These materials will allow you to leverage the high tensile strength and low hydrogen properties of the E11018M electrode effectively in your PQR and WPS.
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKH3OmsW3nWAe-OfYKXNeZyk%2BX70RJn87BPrgeYG74s%2BCP4Ueg%40mail.gmail.com.