EBW in titanium for T>50mm

30 views
Skip to first unread message

Hrushikesh Sangamnerkar

unread,
Jul 25, 2015, 12:44:59 AM7/25/15
to material...@googlegroups.com

Gm all,
Anyone experienced in EBW of titanium?
Pl share. Suggest any vendor who has this facility, if any.

Hrushikesh H Sangamnerkar

Muthukrishnan Sivaramakrishnan

unread,
Jul 25, 2015, 2:50:40 AM7/25/15
to material...@googlegroups.com
Dear Mr.Hrushikesh,

 BARC ,Bombay , DRDL ,Hydrabad and GTRI ,Bangalore have EBW facility .Please contact them .

Regards,
S.Muthukrishnan

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMpWL2qQB-GG%2BMqqSvZsP1u%2Ba1y1wT-6Ha-QXvs1JT8fHcdpzQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

SENTHILKUMAR SWAMINATHAN

unread,
Jul 25, 2015, 4:35:43 AM7/25/15
to material...@googlegroups.com
In addition to above locations, WRI - BHEL Trichy has EBW.  
Regards,
S.SENTHILKUMAR



Muthukrishnan Sivaramakrishnan

unread,
Jul 26, 2015, 12:49:21 AM7/26/15
to material...@googlegroups.com
WRI EBW machine was installed by me about 35 years back .It is not in operation now .

muthukrishnan

Shamal Daw

unread,
Jul 26, 2015, 4:53:53 AM7/26/15
to material...@googlegroups.com
Hi

Am not sure but KELTEC ( now BRAMOS)at Trivandrum , Kerala  had this facility .

Kr
Shyam  

Sent from my iPhone

Hrushikesh Sangamnerkar

unread,
Jul 26, 2015, 10:43:30 AM7/26/15
to material...@googlegroups.com

I have shell Dia. Of 3-4 meters. Are they doing EBW with the above mentioned diameter also?

Hrushikesh H Sangamnerkar

Muthukrishnan Sivaramakrishnan

unread,
Jul 27, 2015, 1:20:19 AM7/27/15
to material...@googlegroups.com
Dear Mr.Sangamnerkar,

I doubt about the capabilities of EBWs available in India to meet your demand .For 3 to 4 meter diameter you have to use partial vacuum EBW system which works in open air .Such a facility was demonstrated by SCIAKY ,Frnace in 1776 if I remember correctly during my training at this facility and I participated in this programme. We welded 80 mm thich SS 316 vessel of dia same as yours .In this system the EBW gun will move along the vessel covering the joint area with a special partial vacuum system . OSAKA university people developed another machine in which the vessel is kept in a vacuum room and the beam is impinged on the vessel mounted on a rotary positioner .

For your immediate use please use normal TIG welding and a roller positioner rotate the vessel. Please inform your location ,vessel dimensions and code requirement .If you need an welding expert to visit you for procedure qualification with TIG please inform .

Regards,
S.Muthukrishnan

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.

Hrushikesh Sangamnerkar

unread,
Jul 27, 2015, 9:14:01 AM7/27/15
to material...@googlegroups.com

Sir,
Thank you for this information. As far as GTAW is concerned we have much of expertise.

We had also enquired at DRDL,HAL etc. But they regreted.

For BARC, haven't enquired as I didnt get any contact. If u have any pl share.

If that also doesn't work, what u suggest? I think SAW to be carried.

Thank you.

Hrushikesh H Sangamnerkar

SENTHILKUMAR SWAMINATHAN

unread,
Jul 28, 2015, 6:23:16 AM7/28/15
to material...@googlegroups.com
If I remember correctly, L&T Hazira did titanium matl heat  exchanger, wall thickness 9 or 12 mm in 1995 in light fabrication shop with TIG process.
Regards,
S.SENTHILKUMAR



Muthukrishnan Sivaramakrishnan

unread,
Jul 28, 2015, 6:23:49 AM7/28/15
to material...@googlegroups.com
Dear Mr.Sangamnerkar,

As a last attempt consult BHPV ,Vizag .They were working on Titanium .There was one firm presently called TEAM at Trichy started by Dr.Krishnamurthy Rao .They were doing some work in Titanium . You could ask WRI ,BHEL,Trichy for assistance. If you don't find any help please send your requirement and location ,I will check with an expert in this field living at Bangalore and seek his help if he is free.

Regards,
S.Muthukrishnan