Please qualify separately in 2G and 5G to have the welder qualified for all positions.
Thanks.
Pradip Goswami.P.Eng, IWE.
Independent Consulting Welding & Metallurgical Engineering Specialist
Saudi Aramco Approved Designated Project Welding Engineer(DPWR)
Qatar Petroleum Approved, SME-Materials & Corrosion Engineering.
Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/
Email:pgos...@rogers.com,pradip....@gmail.com
Cell/Whasapp:1-905-9793232
From: Hany Nabil <eng.han...@gmail.com>
Sent: May 30, 2021 3:15 AM
To: material...@googlegroups.com
Subject: welder qualification
Dear All,
It is known that the 6G position qualifies welder for all positions.
If not possible to apply for a 6G position during WQT what are the two positions necessary to qualify a welder for all positions ?
Best Regards,
Eng. Hany Nabi
Welding Engineer
Email: eng.han...@gmail.com
Egypt Mobile: 002-01225622022
This message, including any attachments, may contain confidential and privileged information for the sole use of the intended recipient(s). Review, use, distribution or disclosure by others is strictly prohibited. If you are not the intended recipient, or authorized to receive information on behalf of the recipient, please contact the sender by reply email, and delete all copies of this message. While we have taken reasonable precautions to ensure that this message and any attachments are free from viruses, we cannot guarantee that they are virus free and accept no liability for any damage caused by this message or any attachments. Messages sent or received through our networks may be monitored to ensure compliance with the law, regulation and/or our policies.
Dear All,
It is known that the 6G position qualifies welder for all positions.
If not possible to apply for a 6G position during WQT what are the two positions necessary to qualify a welder for all positions ?--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP1YJmRDNM44i9pQKAFGrp33_%3DfOZD7eror1ugpaunNLcFmvYw%40mail.gmail.com.
--
J.Gerald Jayakumar