Dear Experts,
Need your expert advice on following subject matter.
We want to seal weld between these dissimilar metal for elimination of leakage.
Kindly suggest recommended
filler Wire & weld parameter for the same.
Thanks & regards,
Brajendra Patel
Cont:+917057406907
Hi Brajendra,
According to Matweb, Haynes has discontinued his product. Hence very little information is available in the web. Feel free to share the OEM’s specifications or data sheet for better clarity of the problem.
Between these 2 alloys, D-205 is more austenitic, containing more Nickel. Hence recommended welding filler for this alloy should be default choice for welding between these 2 alloys.
Thanks.
P.Goswami.P.Eng, IWE.
Welding & Metallurgical Specialist
Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2Bi%2BCirf9wVr4kKJ_bQ38Un1Sg1s8my387XU%3Ddqfg0rFQpcuFQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.