Welder qualification

117 views
Skip to first unread message

Krisanu Bhunia

unread,
Aug 21, 2016, 6:39:30 AM8/21/16
to material...@googlegroups.com
Daer.ALL
Please tell me cluster porosity acceptance limit for Welder qualification test as per ASME XI or VII.

 Regards
krisanu bhunia

Sathish Kumar

unread,
Aug 21, 2016, 11:18:34 PM8/21/16
to material...@googlegroups.com

Dear Krisanu Bhunia and Experts,


FOR WELDER QUALIFICATION TEST


I would like to share my experience as below, ( correct me if I am wrong. )


From Quality point of View:

·         First thing is “ Welder qualification test” is done to determine the ability of a welder

to deposit sound weld metal.

·         Sound metal means a quality weld at first time. ( without making visual defects like cracks, undercuts, porosity, excess reinforcement, Etc. )

·         As per ASME SEC IX, the only visual criteria you could find as mentioned below:

·         QW-194 Visual Examination — Performance

Performance test coupons shall show complete joint

penetration with complete fusion of weld metal and base

metal.


From Production Point of View: -  During the test, If a welder making undercut or with Visual porosity – please reject him, before your client does the same, since this welder if qualified  - he will make more undercuts and porosity in the Job and uses grinder repeatedly / wastes precious time schedule of the project / off course increase the work of Welding Inspector and cannot make a productive output results. Hope you got the message.


AND FINALLY – Client have to decide !


Regards,


Sathish

Jazan, Saudi.


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMZth3rV_ULUn4hEhHvtKAKuzQD5i4t5sFXcCZvZ%3DWHZQN40mA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

anand gupta

unread,
Aug 21, 2016, 11:19:05 PM8/21/16
to material...@googlegroups.com
Dear
For welder test piece must be free from all defects.

a p gupta
baroda


On Sun, 21 Aug, 2016 at 0:12, Krisanu Bhunia
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.

Mukkaish K

unread,
Aug 23, 2016, 12:16:24 AM8/23/16
to Materials & Welding
Dear Krisanu Bhunia, 

Refer to clause no. QW-191.1.2.2 (b) (3) Qualification Test Welds of the ASME Sec IX - 2015 -- Assuming test coupon is greater than 3 mm.
You can get the acceptance criteria for cluster porosity.


Regards
MK

Krisanu Bhunia

unread,
Aug 23, 2016, 2:25:01 AM8/23/16
to Materials & Welding
Thank for information.
But for cluster porosity in radiography have any accepting limitations or not ?
What is the limitations if it have ?

ammar maghami

unread,
Aug 24, 2016, 2:00:59 AM8/24/16
to material...@googlegroups.com
Dear krisanu

Hi

For cluster porosity  acceptance criteria you must characterized the type of material and specification and then interpretation this imperfection.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Reply all
Reply to author
Forward
0 new messages