Dear Experts, 

As per standards how many year after vacuum pack electrode expiry  

Regards

VINOD.

Dinesh Somwanshi

未読、
2019/08/12 5:01:052019/08/12
To: materials-welding


Supplier recommending for 6 years.

Thanks & Regards

DINESH VITTHAL SOMWANSHI

असो द्यावी दया तुमच्या लागतसे पाया.

*Pray for others, sometime, You might never need to pray for yourself
again.....*



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BfkJkskQLEUi6J_GZLbhXH3TfukHkkPzTn1dFfVYDyE5sc4gg%40mail.gmail.com.

munee...@gmail.com

未読、
2019/08/12 23:24:552019/08/12
To: materials-welding
Hi,

Electrode expiry, which is shelf life comes with manufacturing recommendations, but still some debate asking that ''whether its a food item to have expiry'' its not but it has shelf life which may differ 3 or 4 years as per manufacturer recommendations, and can be continued if stored in proper condition if your manufacturer accepts.

So at any case check the manufacturer recommendation and if exceed take a concurrnece from manufacturer and satisfy your client with continous proper storage records, because in any case of serious or pattern defects, before the question arises, have a proof, this shall be ongoing observation as a part of quality focus assesments.

Below is one of the australian manufacturer for electrodes, where i had to concur as proactive.


Regards,

Muneeb.