Hello Rahim,
It depends on your client!
Few reputed clients accept ASME Section 09 WPS in place of AWS D1.1.You can convinces your client by referring to API RP 582 - 2nd Edition, Clause 4.
Before approaching your client ,please ensure API RP 582 is applicable for the project.
4 General Welding Requirements
4.1 Structural (nonpressure boundary) welding requirements shall comply with either AWS D1.1 or AWS D1.6.
When approved by the purchaser (engineer) welding procedures may be qualified per ASME BPVC Section IX.”
Thanks and regards,
Sudhakar.K