For your applications:
1. Polysoude P6 + MU IV Open Head + Cold Wire—Suitable for SS 25 NB to 300 NB and 2–10 mm wall thickness.
2. AXXAIR SAXX 300 + Open Head—An alternative with a user-friendly interface.
Both brands are available in the commercial market and may cost between 20 and 50 lakhs, depending on the
configuration.
Your 10 mm thick and 300 NB size requires an open-head or carriage-type orbital system with a wire feed.
A closed head is ideal for thin-wall tubing.
Equipment Configuration should have:
Inverter orbital power source
Open orbital welding head
AVC (Arc Voltage Control)
Torch oscillation
Cold wire feeder
Water cooling
Weld data logger
Oxygen analyser (for purge monitoring)
Internal pipe purging system
Remote pendant
Weld procedure memory (at least 200 to 300 programs)
Both systems are good for dairy, pharma, food processing, and SS fabrication. If you have any other brand in
mind, please go ahead.
C Sridhar.
------------------------------------------------------------------------------------------------------------------------------------------------
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/5a3bf8d7-b258-4a6e-aa65-678704845196n%40googlegroups.com.
Lincoln Electric – STT mechanised pipeline systems.
Fronius – CMT mechanised pipeline systems.
CRC-Evans – Integrated automatic pipeline welding systems.
Serimax – Premium offshore pipeline welding systems.
are generally recommended.
These companies work through project-based sales and engineering support rather than stocking equipment
through conventional dealers.
C Sridhar.
Regards,
Ashish Ranjan
![]()
Save a tree...Please consider your environmental responsibility. Before printing this e-mail message, ask yourself whether you really need a hardcopy.
"Confidentiality Warning: This message and any attachments are intended only for the use of the intended recipient(s), are confidential and may be privileged. If you are not the intended recipient, you are hereby notified that any review, re-transmission, conversion to hard copy, copying, circulation or other use of this message and any attachments is strictly prohibited. If you are not the intended recipient, please notify the sender immediately by return email and delete this message and any attachments from your system.
Virus Warning: Although the company has taken reasonable precautions to ensure no viruses are present in this email. The company cannot accept responsibility for any loss or damage arising from the use of this email or attachment."
Caution: The e-mail below is from an external source. Please do not open attachments or click links unless this email comes from a known sender and you know the content is safe. |
| Polysoude | P4/P6 family + appropriate open/carriage heads | Excellent | Excellent | ⭐⭐⭐⭐⭐ |
| Orbitalum | Orbital TIG power source + HX/pipe heads | Very good | Excellent | ⭐⭐⭐⭐⭐ |
| AXXAIR | Orbital TIG systems + open heads | Very good | Very good | ⭐⭐⭐⭐½ |
| AMI | Model 207/415-type orbital systems + suitable heads | Very good | Excellent | ⭐⭐⭐⭐½ |
Regards,
Ashish Ranjan
![]()
Save a tree...Please consider your environmental responsibility. Before printing this e-mail message, ask yourself whether you really need a hardcopy.
"Confidentiality Warning: This message and any attachments are intended only for the use of the intended recipient(s), are confidential and may be privileged. If you are not the intended recipient, you are hereby notified that any review, re-transmission, conversion to hard copy, copying, circulation or other use of this message and any attachments is strictly prohibited. If you are not the intended recipient, please notify the sender immediately by return email and delete this message and any attachments from your system.
Virus Warning: Although the company has taken reasonable precautions to ensure no viruses are present in this email. The company cannot accept responsibility for any loss or damage arising from the use of this email or attachment."
Caution: The e-mail below is from an external source. Please do not open attachments or click links unless this email comes from a known sender and you know the content is safe. |