Groups
Groups
Sign in
Groups
Groups
Materials & Welding
Conversations
Labels
About
Send feedback
Help
How many coupons needed for welders qualifications of welder from 2'' (OD:60.33 mm) SCH : 5.18 mm ) GTAW according to ASME SEC.IX.
59 views
Skip to first unread message
Raja kumarasamy
unread,
Aug 5, 2019, 9:40:07 AM
8/5/19
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to Materials & Welding, material...@googlegroups.com, Ilangkumaran Kumarasamy, Kumar Kumar, Karthik
Dear sirs,
How many coupons needed for welders qualifications of welder from 2'' (OD:60.33 mm) SCH : 5.18 mm ) GTAW according to ASME SEC.IX.
Regards
Raja kumarasamy
Welding & Piping inspector
ADNOC Waste Heat Recovery Project
Ruwais, Abudhabi
UAE
Mobile
:
+971-565495293
INDIA
Mobile
:
+91-9487403889
Karthik
unread,
Aug 6, 2019, 12:03:37 AM
8/6/19
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to Materials & Welding, material...@googlegroups.com, Ilangkumaran Kumarasamy, Kumar Kumar
Hi,
1 coupon for 2" OD pipe. (As per Sec.IX; QW303.2, Minimum length of coupon to be examined is 150mm)
Thanks& Regards,
(Karthik)
Karthikeyan.S
QA/QC Manager
Agon Pacific Co.,Ltd.
M: +66-655-174-397, +66-892-512-282
E-mail : k
arthi...@yahoo.com
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-weld...@googlegroups.com
.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/1308484406.1069275.1565010887764%40mail.yahoo.com
.
anthony chundal
unread,
Aug 6, 2019, 12:03:37 AM
8/6/19
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to material...@googlegroups.com, material...@googlegroups.com, Ilangkumaran Kumarasamy, Kumar Kumar, Karthik
Dear,
One coupon is enough, as the length required for radiography is 150mm,
Regards,
Anthony
Sumit Baliram Bhadakwad
unread,
Aug 7, 2019, 12:41:04 AM
8/7/19
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to Materials & Welding
Hello ,
1 coupon for 2" OD pipe 60 is enough as per given in code
As per Sec.IX; QW303.2,
Regards
Sumit Bhadakwad
Welding & Piping inspector
Pune , India
Vinay Thattey
unread,
Aug 25, 2019, 10:41:34 PM
8/25/19
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to material...@googlegroups.com
Have you observed any issue or failure with first coupen ?
Reply all
Reply to author
Forward
0 new messages