Hope you are doing well and your family and hope that normalcy came back as soon as possible.

Recently, I have been informed about the degradation of the allowable stress of 9Cr materials probably according to the July 2019 publication letter of ASME Section II part D.
I don't have any news about the actual allowable stress, pressure and temperature dependent and I wonder if it is so what is the updated LMP chart. Many facilities which use in their furnace, exchanger and pressure vessel a high temperature resistant steel such as 9Cr material, should be concerned with this issue.

Thank you in advance for your usual understanding and involvement in sharing very important key information with us.

Best regards,
Mostafa,

Vinay Thattey

unread,
Jun 14, 2020, 12:09:35 PM6/14/20
to material...@googlegroups.com
Dear I have not checked it and therefore at present not able to comment .

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/74049505-7f67-41b8-a9c8-11247a727735o%40googlegroups.com.

HENNING John

unread,
Jun 15, 2020, 11:36:39 AM6/15/20
to material...@googlegroups.com

Grade 91 allowables were reduced in ASME 2019 part D in the creep range.

You will need to access the Code to find out the particulars as this is copywrited material.

 

Enjoy.

DISCLAIMER This e-mail and any attachments thereto may contain information which is confidential and/or protected by intellectual property rights and are intended for the sole use of the recipient(s)named above. Any use of the information contained herein (including, but not limited to, total or partial reproduction, communication or distribution in any form) by persons other than the designated recipient(s) is prohibited. If you have received this e-mail in error, please notify the sender either by telephone or by e-mail and delete the material from any computer.
General Data Protection Regulation (GDPR)
We respect and protect your privacy to provide you with our services. Please read https://www.hamon.com/customer-data-protection-notice (Customer) and https://www.hamon.com/seller-data-protection-notice (Supplier) how we process your personal data.

Thank you for your cooperation.
______________________________________________________________________
Reply all
Reply to author
Forward
0 new messages