Dear Friends ; For some technical reasons the expected ferrite after completion of circumferential welding for SS to SS ( ASTM-A -240 SS 316 rolled pipe ) is 7 to 8 . We R using 308L / 316 L filler and obtained result is max 5 . pl advice .
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BQ29OgXQ2ATLV_n9N02pM9cxzYKuCpGX0ah9698DdhMVgOPmg%40mail.gmail.com.
Dear Friends ; For some technical reasons the expected ferrite after completion of circumferential welding for SS to SS ( ASTM-A -240 SS 316 rolled pipe ) is 7 to 8 . We R using 308L / 316 L filler and obtained result is max 5 . pl advice .
--
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEagfUiaQy25n1vxyLMx_C%2B-voUTSmnQSk5Q8tUUUxKn0x64KQ%40mail.gmail.com.