If one welder qualified in CS, possible to weld SS and Low alloy
Karthik
unread,
Jun 23, 2020, 11:25:33 PM6/23/20
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Sign in to report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to Materials & Welding
Hi, Regarding Base material qualification is OK (But please refer QW 423.1) For Filler metal,position etc., please refer ASME Sec.IX-QW 350,351, Table QW-352 to 357 for essential variables for welder qualification and QW-360 to QW-363 for Welding Operator Qualifications. Thanks& Regards,