Hii , can you please tell me about aluminum raw materials (Plate) sampling which BSEN std is applicable.

Vinay

unread,
Feb 22, 2024, 10:14:24 PM2/22/24
to material...@googlegroups.com
Dear All :
Hitherto we were using EWTh-2 confirming to AWS SFA 5.12 . We are now advised by consultant to opt for EWLa-2 i.e .2 % lanthanated Tungsten electrodes .. Any experience by experts and which standard it qua

On Tue, 30 Jan 2024 at 12:29, md.az...@gmail.com <md.az...@gmail.com> wrote:
Hii , can you please tell me about aluminum raw materials (Plate) sampling which BSEN std is applicable.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/12342641-2464-41c7-bf67-ec8f027bd565n%40googlegroups.com.
Reply all
Reply to author
Forward
0 new messages