I am making welds for some pipeline projects in which all are linear welds
and some are different joints but all are fillet welds. For all fillet welds, I am having doubt ❓ about the Welder performance weld repair rate as per codes
In SAEP 324 linear is 0.2 percentage
Saes W10 linear is 2.0 percentage
can anyone tell me the exact repair rate percentage in my case as per the code or reference I need to understand the client with reference?