HOW TO CHOOSE WELDING ROD FOR DIFFERENT MATERIALS

293 views
Skip to first unread message

SURESH KUMAR TS

unread,
Jul 6, 2020, 1:05:41 AM7/6/20
to Materials & Welding
Dear All,

Please can you suggest how to choose the filler material for the different material,

what are all the basic things we need to know: 
if you guide and share with an example what you are following 
it will be of great help.  

Any app your using for searching the filler rod, dear all please share your thoughts on this topic will be great help to other as well. 

Thanks in Advance 
Suresh Kumar TS



Raja Varman

unread,
Jul 6, 2020, 1:23:41 AM7/6/20
to material...@googlegroups.com
To choose filler rod,

Make a table of
Chemical and mechanical properties...
Try to find the highest grade materials,

Choose the electrode properties which next higher level than parent meterials.

Also, consider the another materials property also.

Normally online website are aavailable to choose the electrode.
Try that also

என்றும் அன்புடன்,
Thanks & Regards,
RAJAVARMAN
+971561895584

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c66ec19c-59a1-4543-b90a-c7e3704a1b86n%40googlegroups.com.

SURESH KUMAR TS

unread,
Jul 6, 2020, 2:33:04 AM7/6/20
to Materials & Welding
Dear Sir, 

Thank you for the response.

lets go in detail , i will quote a example, to start with, i need to weld from material SS-304 to material SS-304,

what are all the consideration we need to look in to, 
As you suggested first we need start from material mechanical and chemical properties.
presently what are the ways you recommend, is there a common pool (like website or any specific recommendation of material brand website for referring data sheet) for checking the details or we just google it any random results can be used. 
if you could suggest ... any books & website that we can refer for mention any material we can get the mechanical and chemical properties. 

screen shot of material properties 




Thanks & Regards
Suresh Kumar TS

Ramesh

unread,
Jul 6, 2020, 3:59:58 AM7/6/20
to material...@googlegroups.com

Dear Suresh

 

There are several consumable suppliers that have many recommendations and enough research done on the selection of filler metals to suit your job requirements. 

You need to choose from their catalogue / guideline books. As a sample, attached herewith some guidelines for your reference. Likewise, you can enquire to your consumable supplier for your base metal requirements too.

 

Though many recommendations available, as a welding engineer , you can test for the suitability ( PQR ), Refer as per ASME Sec II-C SFA-5.01M/SFA-5.01 for the consumable procurement guideline, upon successful qualification you can use the selected consumable for your job.

 

Factors to be considered during selection of consumable,

The base material to be welded ( chemistry, Mech property match etc. )

The welding position ( Suitability )

Regulatory specifications and codes ( as per design code )

Design requirements ( impact )

Post-weld heat treatment etc.… 

Thanks and Regards

Rameshkannan Devaraj

"What you have learned is a mere handful; What you haven't learned is the size of the world – Avvaiyar"



ESAB_All _Consumable.pdf
Lincoln Electric all_ product.pdf

Sandeep Pr

unread,
Jul 6, 2020, 4:00:02 AM7/6/20
to material...@googlegroups.com
Dear Friend,


Please Refer AWS D1.6 table 5.3 for your guidance.(For SS)



With Regards,

Sandeep.P.Raghavan


vinu raveendran

unread,
Jul 7, 2020, 1:29:21 AM7/7/20
to Materials & Welding
Dear Suresh,

Refer API 577, Annexure D for selection of consumables with base metal

José Juan Jiménez Alejandro

unread,
Jul 7, 2020, 11:15:11 PM7/7/20
to material...@googlegroups.com
On the internet you can find tables where they suggest contribution materials, generally these tables are based on the experience of other people in the area.
This table was shared with me in this group.
Regards!.

Libre de virus. www.avast.com

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.


--

Ing. José Juan Jiménez Alejandro

Independent Consultant in Parts

and Pressure Equipment

SSI-TPI

Móvil +52 1 812 352 4606

Skype: jjjimeneza






Libre de virus. www.avast.com
Welding Rod Selection.xls
Reply all