During pull out test in mock up of tube to  tubesheet  joints,
If it is broken from tube then it is acceptable or broken from weld is acceptable?

Pieper QSI

unread,
Jul 15, 2016, 6:14:05 AM7/15/16
to material...@googlegroups.com

Depends on project requirements but normally not location of fracture but minimum pull out load is specified.

 

Met vriendelijke groeten / Best Regards,

 

Herman Pieper

QA-QC Inspector / CSWIP + IWI-C Welding Inspector / IWT / Materials Expert

 

Logo_nieuw_vectorized 60%

Job van der Havestraat 6

8384 DB, Wilhelminaoord

Cell: +31 6 51691215

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BEr1RfwRcTAHB9VpPihWo1vrcS_qd3LLPeOuqvrt17E-AGGgQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

image001.png

amol gengaje

unread,
Jul 26, 2016, 5:31:26 AM7/26/16
to material...@googlegroups.com

Generally pull out test is carried to check strength of tube to tube sheet weld joint. The weld joint shall not break at a load lesser than the specified.

On 15 Jul 2016 08:39, "Chokshi Darshan" <chok...@gmail.com> wrote:

During pull out test in mock up of tube to  tubesheet  joints,
If it is broken from tube then it is acceptable or broken from weld is acceptable?

--
Reply all
Reply to author
Forward
0 new messages