AWS welding engineer exam

81 views
Skip to first unread message

Student

unread,
May 5, 2020, 11:31:14 AM5/5/20
to Materials & Welding
Hello,

In the syllabus for AWS CWEng exam, two surfacing process are mentioned as SW, THSP. Anyone have idea what it is?
Reference AWS B5. 16

José Juan Jiménez Alejandro

unread,
May 5, 2020, 12:18:51 PM5/5/20
to material...@googlegroups.com
SW Stud Welding

THSP stands for Thermal Spraying (welding)

Of the second I am not completely sure
Except for the best opinion of someone else in the group

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3bcd2ac8-808f-408b-ad0b-18cc360819be%40googlegroups.com.


--

Ing. José Juan Jiménez Alejandro

Independent Consultant in Parts

and Pressure Equipment

SSI-TPI

Móvil +52 1 812 352 4606

Skype: jjjimeneza





HENNING John

unread,
May 5, 2020, 12:49:05 PM5/5/20
to material...@googlegroups.com
THSP - a generic term (See AWS A3.0) encompassing all thermal spray processes

SW - per AWS 3.0 is the acronym for "arc stud welding". If specifically used in a surfacing question may refer to surface welding as opposed to thermal spray, i.e. conventional welding processes such as SAW.

Enjoy - hope this helps.
--
https://urldefense.proofpoint.com/v2/url?u=https-3A__materials-2Dwelding.blogspot.com_&d=DwIBaQ&c=7jZ8150CN3NzstHYJN0EJg&r=NnjQ8-8YHcs4zhFVtdMkf1ma9qelQ0iAi23fQaW5oVA&m=XEF1TTOIf9N8YSstAuOvKXuYyzdaBEesblBZtb8vTUc&s=EPaf0MwDfOjtUlJ5xJz2epLgcgu6MS9fetNvD3WP1sE&e=
https://urldefense.proofpoint.com/v2/url?u=https-3A__www.linkedin.com_groups_122787&d=DwIBaQ&c=7jZ8150CN3NzstHYJN0EJg&r=NnjQ8-8YHcs4zhFVtdMkf1ma9qelQ0iAi23fQaW5oVA&m=XEF1TTOIf9N8YSstAuOvKXuYyzdaBEesblBZtb8vTUc&s=8ou79cs9RdH2fOq3t_8MMRwm9aJwhU6HMrrjVTFzShE&e=
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://urldefense.proofpoint.com/v2/url?u=https-3A__groups.google.com_d_msgid_materials-2Dwelding_3bcd2ac8-2D808f-2D408b-2Dad0b-2D18cc360819be-2540googlegroups.com&d=DwIBaQ&c=7jZ8150CN3NzstHYJN0EJg&r=NnjQ8-8YHcs4zhFVtdMkf1ma9qelQ0iAi23fQaW5oVA&m=XEF1TTOIf9N8YSstAuOvKXuYyzdaBEesblBZtb8vTUc&s=fLEzv4oNRMIOa-QFhdi4NanGiXQEHF05RcrW3jW4B5k&e= .

DISCLAIMER This e-mail and any attachments thereto may contain information which is confidential and/or protected by intellectual property rights and are intended for the sole use of the recipient(s)named above. Any use of the information contained herein (including, but not limited to, total or partial reproduction, communication or distribution in any form) by persons other than the designated recipient(s) is prohibited. If you have received this e-mail in error, please notify the sender either by telephone or by e-mail and delete the material from any computer.
General Data Protection Regulation (GDPR)
We respect and protect your privacy to provide you with our services. Please read https://www.hamon.com/customer-data-protection-notice (Customer) and https://www.hamon.com/seller-data-protection-notice (Supplier) how we process your personal data.

Thank you for your cooperation.
______________________________________________________________________

Pipeline Welding

unread,
May 7, 2020, 5:12:57 AM5/7/20
to Materials & Welding
 Thermal Spraying (THSP) is the process of spraying molten metal (alloy or pure)onto a surface to form a coating layer over in it.

Prakash Bontra

QC Manager / Sr. Welding Inspector

On Tuesday, May 5, 2020 at 7:18:51 PM UTC+3, José Juan Jiménez Alejandro wrote:
SW Stud Welding

THSP stands for Thermal Spraying (welding)

Of the second I am not completely sure
Except for the best opinion of someone else in the group

El mar., 5 may. 2020 a las 10:31, Student (<nabe...@gmail.com>) escribió:
Hello,

In the syllabus for AWS CWEng exam, two surfacing process are mentioned as SW, THSP. Anyone have idea what it is?
Reference AWS B5. 16

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@googlegroups.com.
Reply all
Reply to author
Forward
0 new messages