Dear kishor,
Hydrotest condition for the tank made up by API 650 is the requirements of carring out major repair means minimum 12 inch nozzle replacement or addition under the working height of liquid.
It means you don't have to do Hydrotest just do the pneumatic at 15 psig for reinforcement pad.
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALpPUFuH1JPwGPD8PJb1GhEzup3GBkuBFT3uuHsMSQ3Y1Ug3Hw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Sir,
Thank you very much for the information. Also pls let me know the clause in API 650, not to do Hydrotest after modification below 12" nozzle.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABhShnbbwV8OXSTNWJ6f0okv3tj-P-Uiiq6hb%2B1PMaE9rTz%2B3w%40mail.gmail.com.
This clause is in API 653 not in API 650.
3.19 definition of major alteration/major repair.
Regards
Faisal Shahzad Meer
+966
- 553919249
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALpPUFvOAJHX9MTkeLX5_-B%2BBwXq4RibKPnd1q7KKbehxgZZOw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Dear faisal,
I have the same case but is there any need to get any design evaluation for the same modification.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/A09A3236B96A6E4290C41417C8A0147E0ADC5751%40GCC-MAILBOX.gcc.local.
As adding/replacing 10” nozzle is not a major repair so no engineering evaluation is required but please refer 12.3.2 of API 653 Addendum 2012 of fourth Edition for more details.
Faisal Shahzad Meer
+966
- 553919249