Interpass Temp. Max

40 views
Skip to first unread message

P NAVEEN

unread,
May 29, 2024, 4:44:21 AM5/29/24
to Materials & Welding
Hii,

What will be max Interpass temp of E 250 Br material in SMAW process.


Thanks

CHINTUKUMAR GANDHI

unread,
May 30, 2024, 2:13:45 PM5/30/24
to Materials & Welding
You can consider it 315º C as per API RP-582 considering ASME Sec. IX P-No. 1 material.