How to get an approximate idea of the condition of a welding machine just by seeing it? These are kept in a warehouse and there is no way to start them.

Balajirajan Palanisamy

unread,
Jan 30, 2020, 4:21:51 AM1/30/20
to material...@googlegroups.com
Dear Mr. Sharjeel,
   If the machine is new and not used then check the manufacturer certificate. If the machine is used one, check the calibration certificate. If you not find any record then you cannot come to know the condition of machine by physical checking.

Best regards,
P. Balajirajan.

On Thu, Jan 30, 2020 at 10:09 AM sfmech <sharje...@gmail.com> wrote:
How to get an approximate idea of the condition of a welding machine just by seeing it? These are kept in a warehouse and there is no way to start them.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9be88115-88d6-4196-add7-3aaf17d31e8b%40googlegroups.com.
Reply all
Reply to author
Forward
0 new messages