Material Grade for RE-bar

31 views
Skip to first unread message

Mohamed ali

unread,
May 24, 2016, 11:42:56 PM5/24/16
to material...@googlegroups.com
Dear Experts,
 
Our Civil department need to weld Re-bar to Re-bar BS 4449-2005 grade, please help me to find equivalent ASTM standard for find out suitable WPS based on "P" Numbers.


Thanks & Regards,
 
Mohamed Ali Samsudeen

JIJILAL K M

unread,
May 25, 2016, 12:55:26 AM5/25/16
to material...@googlegroups.com
Dear Mohamed,

ASTM A615 grade 60 is the weldable grade re bars similar to BS 4449.


JIJILAL K.M. 
QA/QC Manager,
Thai Jurong Engineering Ltd,
KCE SPP Project,Thailand
#096 786 0129


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1094800771.176064.1464146668236.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

憲正 陳

unread,
May 26, 2016, 12:46:54 AM5/26/16
to material...@googlegroups.com
內嵌影像


寄件者: JIJILAL KM <jijil...@gmail.com> 收件者: material...@googlegroups.com 寄件日期: 2016年5月25日(週三)下午12:32 主旨:回复:[MW:24861]材料牌號為RE-酒吧




親愛的穆罕默德,

ASTM A615級60是焊接等級重新類似於BS 4449條。


JIJILAL  KM 
QA / QC經理,
泰國裕廊工程有限公司,
KCE SPP項目,泰國
#096 786 0129


在2016年5月在10:24,“穆罕默德·阿里·”通過材料與焊接25 < material...@googlegroups.com >寫道:
尊敬的專家,
 
我們的民政部門需要重新焊接桿重新酒吧BS 4449-2005級,請幫我找到找到合適的WPS以“P”號相當於ASTM標準。


感謝和問候,穆罕默德·阿里·Samsudeen
 
- http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm 的意見表達/ exchnaged該組中的成員企業人事的意見和意味著僅用於教育目的,用戶必須考慮自己的決定WRT適用碼/標準/合同文件。 --- 因為你訂閱了谷歌論壇“材料與焊接”組。您收到此消息, 要退訂此論壇並停止從中接收電子郵件,發送電子郵件到材料的焊接+unsub...@googlegroups.com 要在此論壇發帖,請發送電子郵件至material...@googlegroups.com 在網絡上查看此討論 更多選擇,請訪問https://groups.google.com/d/optout









- http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm 的意見表達/ exchnaged該組中的成員企業人事的意見和意味著僅用於教育目的,用戶必須考慮自己的決定WRT適用碼/標準/合同文件。 --- 因為你訂閱了谷歌論壇“材料與焊接”組。您收到此消息, 要退訂此論壇並停止從中接收電子郵件,發送電子郵件到材料的焊接+unsub...@googlegroups.com 要在此論壇發帖,請發送電子郵件至material...@googlegroups.com 在網絡上查看此討論 更多選擇,請訪問https://groups.google.com/d/optout










cheng chen

unread,
May 26, 2016, 12:47:29 AM5/26/16
to Materials & Welding


jijilalkm2於 2016年5月25日星期三 UTC+8下午12時55分26秒寫道:

George Dilintas

unread,
May 27, 2016, 10:55:36 PM5/27/16
to Meghanadh K
You can't allocate Pno to a material if this material is not listed in ASME Section IX.
In that case you record on the WPS the material specification and the WPS is valid only or this spec

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1094800771.176064.1464146668236.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis
Reply all
Reply to author
Forward
0 new messages