Can a welder use SS electrode on CS material ? for qualification and what is the range?
thanks

Ritesh Kumar Singh

unread,
Oct 16, 2023, 3:45:22 AM10/16/23
to material...@googlegroups.com
Mean he is qualified for CS & SS Both. 

On Mon, 16 Oct, 2023, 12:52 pm John, <johnmouni...@gmail.com> wrote:
Can a welder use SS electrode on CS material ? for qualification and what is the range?
thanks

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/96f58af9-2886-4359-99c7-b6ff1faddbc6n%40googlegroups.com.

Suraj Naik (KPCL)

unread,
Oct 24, 2023, 9:12:37 AM10/24/23
to material...@googlegroups.com
Dear Ritesh,
It is depend on P No. & F No and P No. of SS and CS is different so that it is not applicable for do welding vice versa.


Regards,
Suraj Naik




--
Thanks & Regards
Suraj Naik
Contact- 8956230597



This e-mail and any files transmitted with it are for the sole or exclusive use of the intended recipient(s) and may contain confidential, proprietary and privileged information. If you are not the intended recipient, please contact the sender by reply e-mail and destroy all copies and the original message. Any unauthorized review, use, disclosure, dissemination, forwarding, printing or copying of this email or any action taken in reliance on this e-mail is strictly prohibited and may be unlawful. The recipient acknowledges that Kirloskar Pneumatic Co. Ltd. or its subsidiaries and associated companies are unable to exercise control or ensure or guarantee the integrity of/over the contents of the information contained in e-mail transmissions and further acknowledges that any views expressed in this message are those of the individual sender and no binding nature of the message shall be implied or assumed unless the sender does so expressly with due authority of Kirloskar Pneumatic Co. Ltd. Before opening any attachments please check them for viruses and defects.

WARNING: Computer viruses can be transmitted via email. The recipient should check this email and any attachments for the presence of viruses. The company accepts no liability for any damage caused by any virus transmitted by this email.

Visit us at: www.kirloskarpneumatic.com

Vishwas Keskar

unread,
Oct 24, 2023, 12:01:38 PM10/24/23
to material...@googlegroups.com
Dear John
Your query is not clear 
Pl details out the query with background so that guidance can be given
Sent from my iPhone

On 24-Oct-2023, at 6:42 PM, 'Suraj Naik (KPCL)' via Materials & Welding <material...@googlegroups.com> wrote:



Ramamoorthi Thangarasu

unread,
Oct 24, 2023, 12:01:48 PM10/24/23
to material...@googlegroups.com
Hi 
There are 2 different work operations mixed together.

1) SS electorate not possible for cs materials because the chemical composition was changed.required new PQR/WPS for cs.
2) as per ASME Sec IX SS Welder can be eligible for CS only limitation for piping for (back Purging). 

Regards
Ramamoorthi Thangarasu