Minimum Diameter and Thicknes to perform NDT by UT manual

76 views
Skip to first unread message

richard burthon

unread,
Aug 19, 2016, 10:16:41 PM8/19/16
to Materials & Welding
Dear All,

Please inform me reference and standard, what is minimum diameter and thickness to be able to perform by UT Manual,..?as per ASME V there is no information, as per AWS D.1.1 just only mention thickness from 8 mm to 200 mm, 


thanks

anthony chundal

unread,
Aug 20, 2016, 6:07:43 AM8/20/16
to material...@googlegroups.com
Hi Richard,

As per ASME Sec VIII Div-1, Uw-51, you can do UT from 6mm thk, please find below extract.

Inline image 1

Thanks & Regards,
Anthony.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/931d4b74-0ea4-4ed8-aaaf-0de57542db17%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Reply all
Reply to author
Forward
0 new messages