Gas purity conformation

45 views
Skip to first unread message

JITHIN GOPINATH

unread,
Jun 12, 2023, 6:46:06 AM6/12/23
to material...@googlegroups.com
Sir,
 As per sec IX and API 1104 purity of gas is not an essential variable but in sec II C they had mentioned about the purity percentage. For example I have a gas certificate for CO2 with 99.5% but as per sec II C the purity percentage is given as 99.8%.
 So please advise me can I go with 99.5%...


Thanks and Regards

Jithin 

Vishwas Keskar Welding Manager WELDING

unread,
Jun 13, 2023, 12:23:47 AM6/13/23
to Materials & Welding
You can use 99.5 % 
Pl. qualify PQR and address in WPS as
Shielding Gas - CO2 
Composition - 99.5 % minimum 

In the said case you can NOT write Shielding gas - SFA 5.32  SG-C in WPS ,PQR 

Thanks and regards

Vishwas -IWE 