Hi friend,
As per EN 10204, different designation of classes are their, -
Ex 3.2, it is demanding witness / validation by TPI/Owner is mandatory, in the same STD 2.1, 2.2 Designations are also available – which manufacturers will submit his test reports, complying to other supporting documents.
Hence you can convince to china manufacturers stating that “as per EN 10204 – Designating 2.1 or 2,2”
Also that the material / product is going out of china then the documentation shall also be in accordance to the recipient country standards, because end user requirements has to comply.
Equivalent ISO code is ISO 10474
Thanks & Regards,
Lakshman Kumar B,
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c4293ab0-f13d-4100-aef4-9061e94b7816%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Hi Farzad,
If this standard (EN10204) is mandated in Project specification vendor should ask for deviations at the very beginning, not when equipments or components are getting ready for completion or shipment. That’s unethical.
The salient points of EN10204 3.1 are explained in the attachments. There are many Chinese vendors who are able to meet these overseas standards or else their product will not get exported.
You may require some firm but logical talks with your EPC contractor.
Please see the link from LR’s website also for more clarifications.
Thanks.
Pradip Goswami, P.Eng,IWE
Independent Welding & Metallurgical Engineering Specialist &
Consultant.
Ontario,Canada.
ca.linkedin.com/pub/pradip-goswami/5/985/299
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8fe88b53-0094-48d8-a0ce-3c9f18110390%40googlegroups.com.

To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAYAAAAAAAAAOT5XfyRhstKvyeqQRSrfFXCgAAAEAAAAJ5k5o4rbs1FuCb7fUKMH2oBAAAAAA%3D%3D%40quickclic.net.