Dear master 

please can you advise me i have some doubt 
in our project i have a PQR qualify with gtaw + smaw butt weld 
Detail :
 
7.14 to 20 (CS & LTCS)
GTAW  5 mm +SMAW 9

ER70S-6 + E7018-1 


and i want to qualify to only SMAW PROCESS is it possible or no 



biennd

nepřečteno,
31. 5. 2023 5:17:3931.05.23
komu: Materials & Welding
Hi there,

May you check in which standard refers to.
I understood, ASME IX allowed for thickness of test coupon more than 13 mm.

Thanks
Bien ND

Baqer Shabbeer

nepřečteno,
31. 5. 2023 5:38:1631.05.23
komu: material...@googlegroups.com

Yes its possible, You can go for only SMAW considering all other essential variable

 

QW-200.2(f) One WPS. Several WPSs may be prepared from the data on a single PQR (e.g., a 1G plate PQR may support WPSs for the F, V, H, and O positions on plate or pipe within all other essential variables). A single WPS may cover several sets of essential variable ranges as long as a supporting PQR exists for each essential and, when required, supplementary essential variable [e.g., a single WPS may cover a thickness range from 1/16 in. (1.5 mm) through 11/4 in. (32 mm) if PQRs exist for both the 1/16 in. (1.5 mm) through 3/16 in. (5 mm) and 3/16 in. (5 mm) through 11/4 in. (32 mm) thickness ranges].

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8e67b12e-4012-4530-91ce-7940fb52f5d6n%40googlegroups.com.

paresh patel

nepřečteno,
31. 5. 2023 22:58:2131.05.23
komu: material...@googlegroups.com
You can prepare WPS for SMAW only. considering essential variables.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

Mahesh Rajpurohit

nepřečteno,
8. 6. 2023 2:27:0008.06.23
komu: material...@googlegroups.com
Dear Team 

Kindly suggest me the welding rod material standard used S355 J2 N plate 

And method of welding which is suitable for making round pipe from plate of 25mm Thickness 

Your's 
Mahesh Purohit



Parminder Singh

nepřečteno,
8. 6. 2023 2:51:4308.06.23
komu: material...@googlegroups.com
Dear Sir, 

1. You can use E-7018-1 