Dear All,
 
Can someone give the Reference Standard or clause for Weld Visual Acceptance Criteria as per ASME VIII
 


--
with regards,

Rahoof Hassan,
Abu Dhabi, UAE

Theanh Lai

unread,
Jul 2, 2015, 8:01:54 AM7/2/15
to material...@googlegroups.com
Please see ASME VIII-UW-35 carefully. you will see thing which you need