Regarding qualification as per ASME Sec IX supports the material

36 views
Skip to first unread message

mohit aggarwal

unread,
Jan 18, 2023, 10:06:04 PM1/18/23
to Materials & Welding
Hi Experts,

Greetings!

We have welding of material grade SB 410 with SA 105 (P1 Group 1) & SB 410 to SB 410  as per attached drg.

3rd stage heater (5).bmptubesheet to channel.bmp

SB 410 is not classified in ASME Sec IX. It is classified in JIS G 3103.

I want to know if you have experience or advice can I support ASME Sec IX procedure qualification for this material combination.

If I can't support the existing Procedure from P1 to P1 material combination then what is the way out to qualify this material as per ASME Equivalent or mandatorily I'll have to qualify new procedure for this combination.


Regards,
Mohit Aggarwal
Welding Engineer

Vishwas Keskar Welding Manager WELDING

unread,
Jan 22, 2023, 9:38:01 PM1/22/23
to Materials & Welding
what is  SB 410 and what is chemical composition/ MTC ?
Is this job is ASME Stamped Vessel ?
Vishwas -IWE 
Reply all
Reply to author
Forward
0 new messages