Dear sirs,

kindly advise on the below query.....


 Deposited weld metal made using a bare rod not covered by an SFA Specification but which conforms to an analysis listed in Table QW-442 shall be considered to be classified as F‐No. 6.


 Regards
Raja 

Kannayeram Gnanapandithan

unread,
Sep 30, 2019, 5:18:38 AM9/30/19
to materials-welding
F no may not be issues. Only weld metal A no may be issues. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/894699591.406112.1569676100044%40mail.yahoo.com.
Reply all
Reply to author
Forward
0 new messages