Dissiminal welding between aluminum alloy and stainless steel

43 views
Skip to first unread message

duynhat240685 nguyen

unread,
Dec 18, 2016, 9:53:43 PM12/18/16
to Materials & Welding
I am researching on the dissimilar welding materials by using TIG and MIG welding method. But I don't know, how to calculate the welding parameters? please help me. 
Thank you so much!

Shashank Vagal

unread,
Dec 18, 2016, 11:21:47 PM12/18/16
to material...@googlegroups.com
Manufacturer's catalogue would be a good start.

Shashank C Vagal




From: duynhat240685 nguyen <duynha...@gmail.com>
To: Materials & Welding <material...@googlegroups.com>
Sent: Monday, 19 December 2016 7:43 AM
Subject: [MW:25830] Dissiminal welding between aluminum alloy and stainless steel

I am researching on the dissimilar welding materials by using TIG and MIG welding method. But I don't know, how to calculate the welding parameters? please help me. 
Thank you so much!
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/dc3dab79-6d6d-4be5-a0bf-c45aea50abdc%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


dilintas

unread,
Dec 19, 2016, 5:37:38 AM12/19/16
to Meghanadh K
Not possible.
You may use intermediate piece fabricated by explosion bonding or sintering



Sent from my Samsung Galaxy smartphone.

Tijo Mathew

unread,
Jan 5, 2017, 12:38:58 AM1/5/17
to Materials & Welding
You may use friction stir welding
Reply all