SP0472 STANDARD - WPS

274 views
Skip to first unread message

Vishwas Keskar Welding Manager WELDING

unread,
Jul 5, 2020, 3:07:21 AM7/5/20
to Materials & Welding
WPS is prepared without PWHT with HARDNESS check in PQR  .
It meets Hardness less than 248Hv10  along CE requirements as per  SP0472

Std states that  hardness Control shall be 
1)  CE control 
  and THERMAL TREATMENT - We intent to apply t8/5  concept.

We have to incorporate  t8/5 in WPS   as per Customer advice .

Can somebody throw light on SP0472 and t8/5 cooling time  requirements / concept . How it is to be applied theoretically as well as practically during production usage


Charles Jacob

unread,
Jul 5, 2020, 4:11:39 AM7/5/20
to material...@googlegroups.com
Dear vishal,

Pl follow EN 1011-2. It gives complete details of welding requirements for steel. 


Regards,
Charles 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/87e9f198-abde-4b90-bb53-1fab636bd33bo%40googlegroups.com.

pgos...@rogers.com

unread,
Jul 5, 2020, 11:19:50 PM7/5/20
to material...@googlegroups.com

Hello Vishwas,

 

Please see the appropriate extracts from NACE SP-0472 for your information. Appendix C Summary of Cooling Time (t8/5) Concept is purely theorical. The explanations are clarified in the relevant text and figures. Yes a combination of preheat, control of inter pass temperature 2 dimensional vs 3 dimensional heat flow all are important factors to control hardness.  The hardness requirements as per this document is clarified in Section -2 (as attached).

 

Note SP-0472 is not a design document. It’s more of a supportive document to MR-0103. Hence for WPS/PQR qualifications one has to fulfil the requirements of MR-0103 ( when indicated in the contract)  and SP-0472 only for the hardness control.

 

Your query does not state the design requirements. If the hardness of 248 HV10 meets the design requirements then the PQR should be accepted , provided all the welding control as per SP-0472 are fulfilled.

 

Thanks.

 

 

Pradip Goswami, P.Eng, IWE

Consultant-Welding-Metallurgical Engineering

Cell & Whatsapp-905-9793232.

Personal:pradip....@gmail.com

 

 

From: material...@googlegroups.com <material...@googlegroups.com> On Behalf Of Charles Jacob
Sent: July 5, 2020 3:21 AM
To: material...@googlegroups.com
Subject: Re: [MW:31097] SP0472 STANDARD - WPS

 

Dear vishal,

 

Pl follow EN 1011-2. It gives complete details of welding requirements for steel. Summary of Cooling Time (t8/5) Concept is a general guidance on how to control cooling rates , in order to avoid

 

 

Regards,

Charles 

Pages from NACE SP0472 2015-2.pdf
Pages from NACE SP0472 2015.pdf

Vishwas Keskar

unread,
Jul 6, 2020, 4:50:26 AM7/6/20
to material...@googlegroups.com
THANK YOU  ALL FOR RESPONSE .
 PL elaborate  following :
When  minimum T8/5  time is calculated   using SP472 formulae  for  PQR , then  how it is to be applied  for production welds ?
 There are various  diameter / thk involved in production.The WPS( thk etc) is  is covering production welds


You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/8Y6H3Kbz1VY/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAuAAAAAAAAABVPzeizzeRJsiPziIE5jXQBAMO2jhD3dRHOtM0AqgC7tuYAAAAAAA4AABAAAAAtPvHm0xMFSLVmbw2psUhXAQAAAAA%3D%40rogers.com.

Vishwas Keskar Welding Manager WELDING

unread,
Apr 15, 2021, 12:54:15 AM4/15/21
to Materials & Welding
thanks experts

I gone thr EN1011 -  ANNEX -  D
Studied equations /figures 
Need following elaborations :
1)How to calculate Transition thickness - Formaulae ? 
2) What is significance of the transition thickness?
3)After calculation , what its use ,how it is to applied  to production joints , calculations
4)How and what to interpret  in Figures of D4, D5, D6 

Vishwas 