Dear all,
        Please suggest API5L X70 GRDE pipeline .Which electrode E7010 or E8010

Muhammad Azeem

unread,
Nov 21, 2022, 6:16:25 AM11/21/22
to material...@googlegroups.com
You can used 7010 root and filling capping 8010..

On Mon, 21 Nov 2022, 13:05 karu...@gmail.com, <karu...@gmail.com> wrote:
Dear all,
        Please suggest API5L X70 GRDE pipeline .Which electrode E7010 or E8010

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8725c287-0d1d-451b-ae7e-551e5bede9f5n%40googlegroups.com.

Karunakaran Karan

unread,
Nov 21, 2022, 10:29:02 PM11/21/22
to material...@googlegroups.com

Kannayeram Gnanapandithan

unread,
Nov 21, 2022, 10:29:02 PM11/21/22
to materials-welding
Reply all
Reply to author
Forward
0 new messages