WPS Supplementary essential variable for Impact

121 views
Skip to first unread message

Chetan

unread,
Aug 13, 2015, 2:12:55 AM8/13/15
to material...@googlegroups.com
Dear sir,

I have PQR for P1 G1 to P1 G2 as per Impact test requirement  G no. is supplementary essential variable.
My question is can I made P1 G1 to P1 G1 & P1 G2 to P1 G2 wps using same PQR without change in other essential & supplementary variable.

solomon

unread,
Aug 13, 2015, 4:20:58 AM8/13/15
to Materials & Welding
Hi Vicky Patil
Your understand is correct if other essential&supplementary variable are met.

เมื่อ วันพฤหัสบดีที่ 13 สิงหาคม ค.ศ. 2015 13 นาฬิกา 12 นาที 55 วินาที UTC+7, vicky patil เขียนว่า:

Mohan Kumar

unread,
Aug 13, 2015, 6:14:53 AM8/13/15
to material...@googlegroups.com
Yes, you can use the same PQR for individual combination. However be sure to perform all the mechanical test including charpies on both base metal side P1 G1 and P1 G2.

Regards
Mohankumar K
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/55cc30cc.4366460a.c86fb.39ea%40mx.google.com.
For more options, visit https://groups.google.com/d/optout.


--
Regards
Mohankumar

Rajnish Dixit

unread,
Aug 13, 2015, 9:00:37 AM8/13/15
to material...@googlegroups.com
Yes, you can make different WPS(s) within the range(s) qualified as per already established PQR if the impact test is not applicable.

When impact test is applicable, all the supplimentary variables will become essential variable and you will have limited provisions to make different WPSs.

Hope, your question is answered.

--------------------------------------------
On Thu, 8/13/15, Chetan <patil...@gmail.com> wrote:

Subject: [MW:23293] WPS Supplementary essential variable for Impact
To: "material...@googlegroups.com" <material...@googlegroups.com>
Date: Thursday, August 13, 2015, 9:52 AM

John Henning

unread,
Aug 13, 2015, 1:03:50 PM8/13/15
to material...@googlegroups.com

Yes, you may.

 

See QW-403.5(c) which reads in part “when base metals of two different P-Number Group Number combinations are qualified using a single test coupon, that coupon qualifies the welding of those two P-Number Group Numbers to themselves as well as to each other using the variables qualified.”

 

Also, as an example see Interpretation IX-15-15:

 

 

From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of Chetan
Sent: Thursday, August 13, 2015 12:53 AM
To: material...@googlegroups.com
Subject: [MW:23293] WPS Supplementary essential variable for Impact

 

Dear sir,



I have PQR for P1 G1 to P1 G2 as per Impact test requirement  G no. is supplementary essential variable.
My question is can I made P1 G1 to P1 G1 & P1 G2 to P1 G2 wps using same PQR without change in other essential & supplementary variable.

--