 For small bore welder test ,Minimum diameter to allow the required nos of test coupon.
Where in Sec IX is stated how much circumference to cover to weld for small bore ( Example 1/2 ") for welder qualification.
Regards
Pradip 

Karthik

unread,
Aug 27, 2015, 12:20:25 AM8/27/15
to material...@googlegroups.com
Hi,
Please refer QW302.2 = ASME Section IX
 
Thanks & Regards,

(Karthik)





--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8m4EWmm30%3Dru01%3DD0U4uVSLXvzkFjpj8by8LQux4mXOkw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


sujin dhas

unread,
Aug 27, 2015, 1:17:57 AM8/27/15
to material...@googlegroups.com
Dear Pradip,

For Welder Performance qualification test, Diameter qualification refer QW-452.3 & QW-452.4

Thickness limits refer QW-452.1(a) & QW-452.1(b)
 
Thanks & Best Regards,
Sujin. J


From: 'Karthik' via Materials & Welding <material...@googlegroups.com>
To: "material...@googlegroups.com" <material...@googlegroups.com>
Sent: Thursday, August 27, 2015 8:15 AM
Subject: Re: [MW:23355] Minimum diameter to allow the required nos of tes

Reply all
Reply to author
Forward
0 new messages