seamless piping and tubing specification SP-TU-002 and/or SP-TU-009
14 views
Skip to first unread message
metmel
unread,
Jul 24, 2019, 11:40:19 PM7/24/19
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to Materials & Welding
Has anyone seen a tubing specification with the designation SP-TU-002? It may be a corporate specification as I can find no other reference than in a Canadian government document.