Material selection for Desalination plants and brine solution

225 views
Skip to first unread message

Hrushikesh Sangamnerkar

unread,
Jul 30, 2019, 11:38:58 AM7/30/19
to Materials & Welding
Dear expert,

Which material is suited to desalination plants keeping in mind the corrosion resistant properties?

Will titanium work well?

If any references or process licensors data available specifically for these applications do share.

Regards,

Hemant W Joshi

unread,
Jul 31, 2019, 3:24:38 AM7/31/19
to material...@googlegroups.com

To shri h. sangamnekar

 

Titanium could be very costly . is the piping meant for raw sea water or the desalinated water?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMpWL2oWhhDc7Db7kUtwjBrNNrZCuY7-nJ%3DLisuw0s80oup9Cw%40mail.gmail.com.

---------------------------------------------------------------------------------------------------------- Information transmitted by this E-MAIL is intended only for the use of the addressee(s) and contains information that is privileged, confidential or exempt from disclosure under applicable law. If you are not the intended recipient or it appears that this mail has been forwarded to you without proper authority, you are notified that any use or dissemination and or copying of this email in any manner is strictly prohibited and you are requested to delete this e-mail immediately. Communicating through e-mail is not secure and capable of interception and delays. Any one communicating with TATA Consulting Engineers Ltd., and / or its subsidiaries or associates or group companies by e-mail accepts the risks involved and their consequences. While this e-mail has been checked for all known viruses, the addressee should also scan for viruses and notify the originator of e-mail. ---------------------------------------------------------------------------------------------------------

rehan khan

unread,
Jul 31, 2019, 4:25:28 AM7/31/19
to material...@googlegroups.com, Hemant W Joshi
Dears,
Titanium is for sea water.                            Thanks & Best   Regards                                                                Rehan

Hrushikesh Sangamnerkar

unread,
Jul 31, 2019, 8:24:43 AM7/31/19
to Materials & Welding

pkra...@gmail.com

unread,
Aug 14, 2019, 7:50:49 AM8/14/19
to Materials & Welding
Can use GRP / Rubber coated steel pipe.

Dhanabal Jalachandran

unread,
Aug 14, 2019, 8:54:44 AM8/14/19
to material...@googlegroups.com

Dear Friend,

 

Stainless steels are the most widely used material in desalination plants. The ideal material for use in desalination plants is titanium because it suffers little to no corrosion in saltwater environments. However, titanium is far more expensive than stainless steels. There are advancements being made to improve the corrosion resistance of stainless steels. Highly alloyed ferritic and austenitic stainless steels are being tested in salt water in comparison to titanium. The stainless steels are normally alloyed with chromium, nickel, molybdenum, and nitrogen to improve their corrosion resistance.

 

Br

Dhanabal Jalachandran

 

Sent from Mail for Windows 10

--

anjansaini

unread,
Aug 16, 2019, 11:13:51 PM8/16/19
to material...@googlegroups.com
CS with rubber lining and monel or non metallic (GRE/FRP/HDPE)
titanium would be costly

Ramin Kondori

unread,
Aug 18, 2019, 8:47:14 AM8/18/19
to material...@googlegroups.com
Duplex grades 


Ramin  Kondori
Sr. QA/QC & Welding Engineer
-----------------------------------------------------------
PG-Dip. in Welding Engineering (IWE  AT  0070)
BSc. in Civil Engineering (IUT)
BGAS Painting Inspector
ASNT Level I&II
                        
IIW-Logo-Colour-small


Vinay Thattey

unread,
Aug 20, 2019, 12:28:40 AM8/20/19
to material...@googlegroups.com
Titanium is a much tougher metal and much more corrosion resistant than stainless steel , however economic aspect with expected life is to be considered for material selection . Its not clear ; what is your end use i.e vessel , pump shaft , bodies , general fabricated structures etc. Duplex steel is also suggested . 
Nickel based alloys like Monel can also be used ( ASTM B 163c , 165 ) .
I suggest pump bodies etc made of duplex steel . For ordinary brine containing vessel Rubber lines CS can also be used .  Remember austenitic SS is not a wonder material .