Dear All

 Anybody knows in which section of ASTM heat treatments methods are defined generally? for example definition of annealing  .

Because we have received a material that must be annealed but after heating it quenched with water.

Regards.

Padmasanker S

unread,
Nov 1, 2015, 11:42:21 PM11/1/15
to material...@googlegroups.com

Hi,

Refer SA-941 of ASMe Sec 2 part b for terminologies...

Best regardz,

Padmasanker
Quality coordinator
Bilfal heavy industries..

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/82d0cae8-98cd-4f61-8f96-a8dbc048c22f%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Reply all
Reply to author
Forward
0 new messages