Pl clarify, how to take hardness measurements on welds after PWHT for SA 516 Gr 70 material.
Is there any code reference?

Thanks& Regards,
Venkatramulu

Rajnish Dixit

unread,
Nov 10, 2019, 3:26:13 AM11/10/19
to materials-welding, ramulu...@gmail.com
Dear Venkat,

Please refer API RP 582 for the same.

Thanks & Best Regards,
Rajnish
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF98%2BdHYCPSu_LL3RaVz%2B7Q10FSw8dED8kXGn_y9oWQyFoTs4A%40mail.gmail.com.
Reply all
Reply to author
Forward
0 new messages