Miter groove weld (ASME B31 3-2018)

841 views
Skip to first unread message

Anna

unread,
Feb 11, 2020, 5:04:29 AM2/11/20
to Materials & Welding

Dear All,


I am a translator of the construction company based in Russia. While studying ASME B31 3-2018 I faced a miter groove weld and don’t quite understand what kind of weld it is and how it looks.


Could anyone please help me?


Thank you in advance.


Best regards, 

Anna 


HENNING John

unread,
Feb 11, 2020, 10:53:50 PM2/11/20
to material...@googlegroups.com

Refers to a fabricated right angle bend.  For a miter joint, the ends of the pipe are cut on 45 degree angle then welded together.  When I worked for a steam turbine manufacturer, we used miter joints in steam piping on the turbine “island” to conserve on space.   (obviously could be any angle but my experience is with 90 degree flow change).

 

Enjoy

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/81ce42de-54d3-4531-9146-7c8e9a740658%40googlegroups.com.

DISCLAIMER This e-mail and any attachments thereto may contain information which is confidential and/or protected by intellectual property rights and are intended for the sole use of the recipient(s)named above. Any use of the information contained herein (including, but not limited to, total or partial reproduction, communication or distribution in any form) by persons other than the designated recipient(s) is prohibited. If you have received this e-mail in error, please notify the sender either by telephone or by e-mail and delete the material from any computer.
General Data Protection Regulation (GDPR)
We respect and protect your privacy to provide you with our services. Please read https://www.hamon.com/customer-data-protection-notice (Customer) and https://www.hamon.com/seller-data-protection-notice (Supplier) how we process your personal data.

Thank you for your cooperation.
______________________________________________________________________

Hemant W Joshi

unread,
Feb 11, 2020, 10:53:55 PM2/11/20
to material...@googlegroups.com

It is your normal butt weld and the miter is a curved portion of a pipe .

--

https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/81ce42de-54d3-4531-9146-7c8e9a740658%40googlegroups.com.

---------------------------------------------------------------------------------------------------------- Information transmitted by this E-MAIL is intended only for the use of the addressee(s) and contains information that is privileged, confidential or exempt from disclosure under applicable law. If you are not the intended recipient or it appears that this mail has been forwarded to you without proper authority, you are notified that any use or dissemination and or copying of this email in any manner is strictly prohibited and you are requested to delete this e-mail immediately. Communicating through e-mail is not secure and capable of interception and delays. Any one communicating with TATA Consulting Engineers Ltd., and / or its subsidiaries or associates or group companies by e-mail accepts the risks involved and their consequences. While this e-mail has been checked for all known viruses, the addressee should also scan for viruses and notify the originator of e-mail. ---------------------------------------------------------------------------------------------------------