HIC Test + NACE

71 views
Skip to first unread message

Vignesh Pal

unread,
Jul 24, 2023, 11:10:11 AM7/24/23
to Materials & Welding
When do we specify HIC requirements along with NACE Sour service requirements?

In many case NACE + HIC are mentioned...what does this mean?

stephen raj

unread,
Aug 2, 2023, 11:41:40 PM8/2/23
to Materials & Welding
Fluid service or exposure to an oilfield environment containing Hydrogen Sulfide (H2S) can cause cracking of materials by damage mechanisms such as SSC / HIC / HSC / SCC /\ SOHIC / SWC / SZC.
Reply all
Reply to author
Forward
0 new messages