Dear Experts,
Kindly suggest consumables for below
Material SA516GR70
Impact @-40C
Impact values – 27J min
Normalizing
Loading – 300C
ROH – 150C
Soaking Temp – 900-920
Soaking Time – 80min
Still Air
SR
Loading – 300C
ROH – 50C max/hr
Soaking – 625C- 645C
Time – 720mins
ROC – 65C max / hr upto 425C
Thank you.