Dear experts,
 i have one question, and I need your help. Thanks first
My WPS is SAW, qualified for tube OD = 2000mm spiral welding pipe sheet pipe.

my WPS is for splicing 2 pipe ( that mean you connecting 2 pipe together )
 the joint design is X bevel
and the layer step of welding is: 
1. GMAW at root
2. cover out side SAW
3. cover inside SAW

so now if I want to change the step welding layer to:
1. GMAW at root
2. cover inside SAW
3.cover out side SAW
 and all other parameters are not change

=>> so my question is . Do I need to requalify my WPS, OR I just rewrite WPS and keep the original PQR,no need to test PQR again


THANKS FOR YOUR HELP.
Jerry.

Ken Waterhouse

unread,
May 23, 2015, 2:29:21 AM5/23/15
to material...@googlegroups.com
Hi Jerry, 

Can you clarify to which code or standard the WPS is written? 

Regards
KW

HAMID HAMIDI

unread,
May 23, 2015, 4:10:34 AM5/23/15
to material...@googlegroups.com
asme sec iiiv qw254 & 255 .no need to retest no problem.



--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/222838b6-bef2-4804-a479-803b7c18cb2f%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


HAMID HAMIDI

unread,
May 23, 2015, 4:30:39 AM5/23/15
to material...@googlegroups.com
im sorry ASME SEC IX QW254&255.




anosh wankhade

unread,
May 23, 2015, 5:01:01 AM5/23/15
to material...@googlegroups.com
Dear Jerry,

In case the WPS is qualified according to ASME section IX, no need to re qualify WPS.

Just make necessary changes in WPS and use to same PQR.

Regards,

Anosh   

For more options, visit https://groups.google.com/d/optout.

Get your own FREE website, FREE domain & FREE mobile app with Company email.  
Know More >

Kannayeram Gnanapandithan

unread,
May 23, 2015, 12:35:43 PM5/23/15
to material...@googlegroups.com

As long as if u are not exceed deposited weldmetal thickness for each process u need not qualify

JERRY TUAN

unread,
May 24, 2015, 11:15:48 PM5/24/15
to material...@googlegroups.com
my code apply is AWS D1.1 for structural steel construction


Thanks Mr Ken Waterhouse.

Vào 13:29:21 UTC+7 Thứ Bảy, ngày 23 tháng 5 năm 2015, Ken Waterhouse đã viết:

JERRY TUAN

unread,
May 24, 2015, 11:15:57 PM5/24/15
to material...@googlegroups.com
my WPS is according to AWS D1.1 . for structural steel construction .

So, if I do not need to test again PQR , I just rewrite welding process layer .

Thanks all experts