90 dig elbow cut in 45 dig

34 views
Skip to first unread message

jamshed...@gmail.com

unread,
Nov 18, 2019, 6:15:31 AM11/18/19
to Materials & Welding
can we cut 90 dig elbow in 45 dig please suggest

dinesh angara

unread,
Nov 18, 2019, 6:40:21 AM11/18/19
to material...@googlegroups.com
yes you can

On Mon, Nov 18, 2019 at 4:45 PM <jamshed...@gmail.com> wrote:
can we cut 90 dig elbow in 45 dig please suggest

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/77b6c2ba-f174-492f-9a40-14a26a641658%40googlegroups.com.

Dinesh Somwanshi

unread,
Nov 19, 2019, 12:29:32 AM11/19/19
to materials-welding
Dear, 

Please get concession request. 

Dinesh





atul khatri

unread,
Nov 19, 2019, 12:29:33 AM11/19/19
to material...@googlegroups.com
you can cut all the odd angles from 90 degree elbows. So just go ahead 

Best Regards
Atul 

On Mon, Nov 18, 2019 at 4:45 PM <jamshed...@gmail.com> wrote:
can we cut 90 dig elbow in 45 dig please suggest

--

haren...@gmail.com

unread,
Nov 19, 2019, 12:29:40 AM11/19/19
to material...@googlegroups.com

Not advisable

--

Jaydeep

unread,
Nov 20, 2019, 11:16:30 PM11/20/19
to Materials & Welding
Yes, You can proceed.