Hello everyone,

I want to weld ArCap material and 306L material together. But I have some problem. I can't achieve a leak-proof seal.

I use laser welding. And The thickness of the 306L material is very low that is 0.6 mm. What should I use as welding wire? I couldn't find it. Or do you have any other suggestions.

Thank you