Dear Sirs
Kindly be informed our specification mandates PWHT on H2S piping classes regardless its material type except on socket weld up to 8mm (wall thickness). my question is what is meant by wall thickness? is it base metal thickness of throat thickness? as you know it'll be differed because thickness of fitting is higher than piping thickness in same schedule.
Kindly clarify the meaning and support us with strong evidence if found.
Regards,
M.Kamel
dili...@gmail.com
unread,
Jul 25, 2016, 9:36:02 AM7/25/16
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to 'Mostafa Kamel Hussein' via Materials & Welding
I would strongly recommend NOT USE socket welds in H2S service. The risk of crevice corrosion is to high