Dear All,
How is olet welded with claded pipe,is there any procedures to follow?

james gerald

unread,
Aug 21, 2022, 3:18:24 AM8/21/22
to material...@googlegroups.com
Please specify below.

1. Run Pipe grade including clad
2. Olet is clad or solid alloy including grade

Thanks & Regards

J.Gerald Jayakumar




On Sunday, 21 August, 2022 at 10:22:49 am GMT+4, TANSON N <tans...@gmail.com> wrote:


Dear All,
How is olet welded with claded pipe,is there any procedures to follow?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/aee9367e-e26e-418b-8255-6eea58c6128cn%40googlegroups.com.

Neilash Kumar

unread,
Aug 23, 2022, 2:28:25 AM8/23/22
to material...@googlegroups.com, TANSON N
Yes before joining the olet to cladded pipe 

Step 1
Buttering on top of pipe face side wall  drilled location .

Step 2 
Grinding using same grade stainless wheel 

Step 3
Etiching using acids to see carbon replaced with stainless steel clad material 

Step 4 cladding and followed with NDT (UT and RT to see the full penetration joint .

Best Regards 
Neilash 

--

Sham Shahabuddin -Welding Inspector, HANBO

unread,
Sep 28, 2022, 3:44:03 AM9/28/22
to material...@googlegroups.com
Dear Sir

Thank you for this knowledge sharing. Can you please mention the reference standards used for this cladding.

Thanks and Regards
SHAM SHAHABUDDIN
QC INSPECTOR - WELDING