Experts please clarify whether one welder can operate two welding machines at a time... It's FCAW process.. Noticed one operator operating two machines... Please clarify is it acceptable or not based on code requirements....
Thanks in advance.....

Ankit Gandhi

unread,
Sep 13, 2016, 7:29:21 AM9/13/16
to Materials & Welding
On Monday, 5 September 2016 15:41:05 UTC+5:30, Govindarajan Shanmugam wrote:
> Experts please clarify whether one welder can operate two welding machines at a time... It's FCAW process.. Noticed one operator operating two machines... Please clarify is it acceptable or not based on code requirements....
> Thanks in advance.....

Dear

I am not sure but we have used two machine by one operator technique for ttj automated process with following ASME.

regards
Ankit Gandhi

c sridhar

unread,
Sep 17, 2016, 8:09:35 AM9/17/16
to material...@googlegroups.com
Yes it is acceptable. Easier if it is a spm or a robotic. 

May not be  practicable it is semi-auto process.

Sridhar.



From: Ankit Gandhi <asgan...@gmail.com>
To: Materials & Welding <material...@googlegroups.com>
Sent: Tuesday, 13 September 2016 2:05 PM
Subject: [MW:25378] Re: One welder operating two welding machined
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsub...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bbb1c541-3a74-4625-80ec-4cc70b7511ce%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


Reply all
Reply to author
Forward
0 new messages