SA 312 TP304 for SA 312 TP 304L

95 views
Skip to first unread message

Dharma dattu

unread,
Jul 7, 2020, 1:29:16 AM7/7/20
to Materials & Welding
Hello All,

We have a new project for which main components are SA 312 TP 304L material, currently we have SA 312 TP 304 WPS can we ues the same, as the Pno. is same!

Regards,
Dharma Dattu. B

Raja Varman

unread,
Jul 7, 2020, 2:49:39 AM7/7/20
to material...@googlegroups.com
Hi.

Both are same P.no8/Group.no1.

So no issue to use the old WPS.
But must be consider,

1. Special requirements other essential variables such as thickness range, 
And supplimentry essential variables,
Based on particular project requirements.

2. Approval of new client.



என்றும் அன்புடன்,
Thanks & Regards,
RAJAVARMAN
+971561895584

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/89ae66ad-2aad-40ce-aed3-fe009c801617o%40googlegroups.com.

wilfred kojo

unread,
Jul 7, 2020, 7:33:18 AM7/7/20
to Materials & Welding
Hi,
You can use since both P-nos and Group nos are the same.

--

Sourav Bohrays

unread,
Jul 7, 2020, 11:15:10 PM7/7/20
to material...@googlegroups.com
yes you can use if there is no requirment of astm a 262 practice e

--

harenath jha

unread,
Jul 7, 2020, 11:15:10 PM7/7/20
to material...@googlegroups.com
Yes you can as per ASME section ix 

Vinay Thattey

unread,
Jul 7, 2020, 11:15:11 PM7/7/20
to material...@googlegroups.com
Yes 

--

Kannayeram Gnanapandithan

unread,
Jul 7, 2020, 11:15:14 PM7/7/20
to materials-welding
Okay. But consumables should have L Carbon

--

Dharma dattu

unread,
Jul 16, 2020, 2:39:25 AM7/16/20
to Materials & Welding
Thanks you all 

Question 1:  WPS was established in 2008, can it be used now?

Question 2: for a 3 meter dia tank how to give purging to do root weld with GTAW.

On Tuesday, 7 July 2020 12:19:39 UTC+5:30, Rajavarman wrote:
Hi.

Both are same P.no8/Group.no1.

So no issue to use the old WPS.
But must be consider,

1. Special requirements other essential variables such as thickness range, 
And supplimentry essential variables,
Based on particular project requirements.

2. Approval of new client.



என்றும் அன்புடன்,
Thanks & Regards,
RAJAVARMAN
+971561895584

On Tue, Jul 7, 2020, 9:29 AM Dharma dattu <dharm...@gmail.com> wrote:
Hello All,

We have a new project for which main components are SA 312 TP 304L material, currently we have SA 312 TP 304 WPS can we ues the same, as the Pno. is same!

Regards,
Dharma Dattu. B

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@googlegroups.com.

Dharma dattu

unread,
Jul 27, 2020, 5:07:37 AM7/27/20
to Materials & Welding
how to give purging for 3 meter dia shell to weld of SA316 Gr 240L material with GMAW (tig).