GAUGE LENGTH REQUIRED SA105 MATERIAL

48 views
Skip to first unread message

Sam

unread,
Jul 26, 2023, 4:25:14 AM7/26/23
to Materials & Welding
Dear Expert,

Gauge length shall be reported in MTC as per ASME SA-105 material. 

Kindly confirm and reference clause.


Thanks,
Sam-Kuwait

james gerald

unread,
Jul 26, 2023, 11:00:04 PM7/26/23
to material...@googlegroups.com
Please refer ASTM A370 or ASME SA-370.

Please also refer ASTM E8M section 6.10

Thanks & Regards

J.Gerald Jayakumar




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/6ce53999-6582-47f4-9399-ae6e7d9da8fdn%40googlegroups.com.
E8M.pdf
Reply all
Reply to author
Forward
0 new messages