Dear Experts,

 Need your opinion  for ERCoCr-E hard facing overlay on A/SA–217 Typ WC6 by PTA Welding Process.

 

1. What shall be weld parameters 

2. Preheat and PWHT requirement (time &  temperature required).

 

Qualification standard is ASME Sec IX.